## Tutorial Description: ###### https://rumble.com/v3vwart-adjusting-eph-20-to-fit-your-needs.html ## Adjusting EPH 20 to Fit Your Needs ## EPH 20 Ingredients: This is EPH 26 but the glass reduced to it's minimum and the "void" is filled with NC. #### Ingredients 11.6 grains LH 11.6 grains LN; 7.5 grains NC (80 to 150) mesh by Rob Yeomans standards) 2.5 grains Glass (150 mesh minimum but 325 mesh is recommended) David Hull uses 3.5 grains Glass (325 Mesh) #### Sparks Adding 1.7 grains of aluminum will produce sparks for rifle rounds and should be more suitable for magnum loads (untested at this time) The aluminum should be between 80-120 mesh (150 tops) to produce sparks.    Otherwise it starts acting like a fuel.  If you desire more fuel - add NC instead.    NC makes for a better fuel because it burns at a lower temperature and produces oxygen while doing so. ### But Wait There's More Vid: [EPH 2x Packing Methods](https://rumble.com/v2f504y-eph-20-powder-packing-methods.html?playlist_id=watch-history)